Qingdao Exceed Fine Chemicals Co.,Ltd

The most professional solution provider of polyurethane and rubber chemicals!

Manufacturer from China
Verified Supplier
6 Years
Home / Products / TDI Based Polyurethane /

Sieve Plate Shore A90 TDI 100 Polyurethane Prepolymer

Contact Now
Qingdao Exceed Fine Chemicals Co.,Ltd
Visit Website
City:qingdao
Province/State:shandong
Country/Region:china
Contact Person:MrLouis.liu
Contact Now

Sieve Plate Shore A90 TDI 100 Polyurethane Prepolymer

Ask Latest Price
Brand Name :EXCEEDCHEM
Model Number :TDI-100/Polyester Polyurethane Prepolymer Shore A90
Certification :ISO9001:2008
Place of Origin :China
MOQ :1mt
Price :FOB Qingdao usd3.0/kg
Payment Terms :L/C, T/T
Supply Ability :3000mt/month
Delivery Time :5-8 work days
Packaging Details :20kg/drum; 200kg/drum
NCO% :4.30-4.50
MOCA% :12.5
Hardness :Shore A90
Base :TDI-100/ polyester based
Packing :20kg/drum; 200kg/drum
Shelf life :6months
more
Contact Now

Add to Cart

Find Similar Videos
View Product Description

TDI-100/Polyester Polyurethane Prepolymer Shore A90

1. Description

This is a TDI-100 based Polyester polyurethane prepolymer.

2. Characteristics

  • High oil resistance
  • Abrasive resistance
  • Good michanical performance

3. Applications

  • Sieve plate
  • Machine parts
  • Sealing ring
  • Roller

4. Typical properties

Type Appearance Viscosity(mPa.s/85℃) NCO% Packing(kg/drum)
Solid 1300-1500 4.30-4.50 20/200

5. Operating Procedure

First, the prepolymer should be preheated in 80-85℃. Second, after vacumming, the prepolymer is to be mixed with melting MOCA evenly. Third, with degassing, casting into mould, and vulcanization,and then demould. Lastly, the finished product should be post vulcanized.

6. Reaction parameters

Item MOCA (%) Gel time(min) Mixing temperature(℃) Post vulcanization(h)
Specification 12.5 8-9 80/120 10

7. Finished products properties

Item Hardness(Shore A) Tensile strength(MPa) Tear strength(KN/m) Rebounding(%)
Physical properties 90 48-50 100-105 36

8. Effects of heating the prepolymer
The isocyanate(NCO) content of all prepolymers decrease with time and especially with exposure to heat. The table below shows the accumulated time taken at various temperatures to degrade prepolymers.
Temperature/℃ Time
60 7 days
70 3 days
80 36 hours
90 12 hours
100 8 hours